I was just trying to help people understand the real problem.

We worked on the bloom for 18 years with a lab, TGA Compounding, different types of ovens ect. And were still unable to cure or make a permanent fix.

What would be helpful is a chart or matrix with Cost, Frequency, Difficulty ect compared. Then people could decide what is best for them without reinventing the wheel each time. Some people would choose a difficult fix over a frequent fix. Or a frequent fix over an expensive one.

I am going to check out your links Kat. But there are 12 of them. It may take a bit.

thanks